Quote:
Originally Posted by CamarosRus
...............And, HOW did you make the Steel Look Correct........?????
|
It would depend on the part. That driveshaft was soaked in eveporust for 24 hours, rinsed, dried & then 0000 steel wool. Stripes painted & then clear coated everything. Some parts needed to go in the blast cabinet. I use black oxide & lower preasure so it doesn't scar the metal. Another thing is I live in southern Az so we don't have the rust problems other states may have. I can't afford what the pros may do so I have to experiment at home....Joe
__________________
1968 Z/28 Corvette Bronze. Black Hounds Tooth. 02E Los Angeles born 3/13/1968 pnt OO
1969 SS396 Yellow/Yellow 08E Norwood born 8/28/1969 pnt 76E
1970 'cuda Moulin Rouge, 440-6, 4 speed
|